Specifications Relating to Shot Peening
(download files in Acrobat pdf format)

The articles below are archived in the shotpeener.com LIBRARY compiled and maintained by Jack Champaigne at Electronics Incorporated.
Visit the LIBRARY to search and access over 3700 abstracts and 2500 full text downloads.
Note: US Specs can be downloaded from the Library free of charge. Others (i.e., SAE, ASTM) must be purchased from the copyright holder.

 

Click on an article title below to view details and access a free full text pdf if available.
Click on column header to re-sort table.

Total articles: 180
TitleYearAuthorSourceAbstract
Cast Shot and Grit Size Specifications for Peening and Cleaning 2012 SAE SAE: J444 SEP2012 RATIONALE During the 2010 revision to this document a typo was made in Figure 1 for S-460 shot screening specification. The 5% max 1.7 mm sieve was changed to the 0% max and the 0...
Peening Media Hardened Steel Peening Balls 2011 SAE SAE: AMS2431/5 REV. B The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS2431...
Cast Shot and Grit Size Specifications for Peening and Cleaning 2010 SAE SAE: J444 JUN2010 RATIONALE Due to NADCAP audit findings on the all pass sieves in Figure 1 and 2 the group is requesting the Figure 1 and 2 all pass changed to 0% and the following be added to the...
Peening Media (ASH), Cast Steel Shot, High Hardness (55 to 62 HRC) 2010 SAE SAE: AMS2431/2 REV. E Revised 2010/12 Superseding AMS2431/2D RATIONALE AMS2431/2E was issued to clarify Table 4 and paragraph 3.9....
Peening Media (ASR), Cast Steel Shot, Regular Hardness (45 to 52 HRC) 2010 SAE SAE: AMS2431/1 REV. E Revised 2010/12 Superseding AMS2431/1D RATIONALE AMS2431/1E was issued to clarify Table 4 and paragraph 3.9...
Rotary Flap Peening of Metal Parts 2010 SAE SAE: AMS2590 Issued 2010-12 This is a new specification that provides technical improvements to MIL-R-81841 in these areas: (1) two methods for determination of intensity independent of peening time, (2) impr...
Flap Assemblies, Rotary Flap Peening 2010 SAE SAE: AS2592 This standard was issued to cover equipment required to accomplish flap peening in accordance with AMS2590....
Peening Media General Requirements 2010 SAE SAE: AMS2431 REV C The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Computer Generated Shot Peening Saturation Curves 2010 SAE SAE: J2597 Jan 2010 The purpose of this recommended practice is to provide an objective method of determining the intensity of peening from a saturation curve. SAE J443 provides instructions for use o...
Chemical Compositions of SAE Carbon Steels 2009 SAE SAE: J403 DEC2009 Issued 1911-06 Revised 2009-12 Superseding J403 NOV2001 RATIONALE a. Table 1 - Based on the grade survey added grades 1002, 1003, 1004, and 1007. Revised footnote 1 in table ...
Shot Peening Coverage Determination 2009 SAE SAE: J2277 Oct2009 This title has been expanded (include word "Determination" to indicate that this standard practice relates to a method of inspection, but does not govern the amount of coverage to ...
Cut Wire Shot 2009 SAE SAE: J441 Nov2009 Cut wire shot shall be the product of carbon steel wire or stainless wire Type 302, 304, Condition B, Spring Temper, cut into the form of cylinders with lengths approximately equal...
Shot Peening, Automatic 2009 SAE SAE: AMS 2430 P Rev. 03/2009 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
General Specification for Removing Organic Coatings from ArmyAircraft using Plastic Media Blasting (PMB) 2008 US Army AMCOM AMCOM US Army MEO A1116D 1.1 Application. a. This section providesthe requirements and procedures for removing organic coatings (paints, primers, or lacquers)and MIL-C-46168, MIL-DT(-53039, and MIL-DTL-64...
Test Strip, Holder and Gage for Shot Peening 2008 SAE SAE: J442 Nov. 2008 This SAE Standard defines requirements for equipment/supplies to be used in measuring shot peening intensity Guidelines for the use of these articles (test strip, holding fixture a...
Shot Peening, Automatic 2008 SAE SAE: AMS 2430 N Rev. 06/2008 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Shot Peening of Metal Parts 2007 SAE SAE AMS-S-13165A RATIONALE AMS-S-13165 has been designated Cancelled and Superseded because equivalent technical requirements are provided by AMS 2430. CANCELLATION NOTICE This specifica...
Peening Media (AWS) Conditioned Stainless Steel Cut Wire Shot 2007 SAE SAE: AMS 2431/4C 05/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (AWCH) Conditioned Carbon Steel Cut Wire Shot, High Hardness (55 to 62 Hrc) AMS 2431 8B 2007 SAE SAE: AMS 2431/8B 05/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media Glass Shot AMS 2431/6C 2007 SAE SAE: AMS 2431/6C 08/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (AWCR) Conditioned Carbon Steel Cut Wire Shot sizes 80, 96, and 116 AMS 2431 3D 2007 SAE SAE: AMS 2431 3D, REV 05/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (ASH) Cast Steel Shot, High Hardness (55 to 62 Hrc) AMS 2431 2D 2007 SAE SAE: AMS 2431 2D, REV 05/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (ASR) Cast Steel Shot, Hard (45 to 52 Hrc) 2007 SAE SAE: AMS 2431 1D, REV 05/01/2007 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media Case Hardened Steel Peening Balls 2006 SAE SAE: AMS 2431/5A 05/2006 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media General Requirements 2006 SAE SAE: AMS 2431B 05/2006 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (AWCH) Conditioned Carbon Steel Cut Wire Shot, High Hardness 2006 SAE SAE: AMS 2431/8A, REV 09/2006 AMS 2431/8A is a Five Year Review and update of this specification....
Peening Media (AWS) Conditioned Stainless Steel Cut Wire Shot, Hard (45 to 50Hrc) AMS 2431 4A 2006 SAE SAE: AMS 2431/4A, REV 05/2006 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (AWRC) Conditioned Carbon Steel Cut Wire Shot, Hard (45 to 52Hrc) AMS 2431 3C 2006 SAE SAE: AMS 2431/3C, REV 02/2002 AMS 2431/3C is a Five Year Review and update for this specification....
AS9101 2006 SAE Aerospace Sae Aerospace AS9101 Rev C 2006-07 This document, AS9101C, has been revised to correct a problem with the scoring formula on page 10, and to include an Appendix B that provides guidance information on audit scoring....
Peening Media Glass Shot AMS 2431/6B 2005 SAE SAE: AMS 2431 6B 02/2005 This specification, in conjunction with the general requirements covered in AMS 2431 establishes the requirements for glass shot to be used for peening of metal parts....
Glass Beads: For Cleaning and Peening 2005 U. S. Specification MIL-PRF-9954B This specification covers glass beads to be used with pressure/suction type blasting equipment....
High Carbon Cast-Steel Shot 2005 SAE SAE: J 827 JUL2005 This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning ...
Cast Shot and Grit Size Specifications for Peening and Cleaning 2005 SAE SAE: J 444 JUL2005 This SAE Recommended Practice pertains to blast cleaning and shot peening and provides for standard cast shot and grit size numbers. For shot, this number corresponds with the ope...
High Carbon Cast-Steel Grit 2005 SAE SAE: J 1993 JUL2005 This SAE Recommended Practice describes the chemical composition, and physical characteristic requirements for high-carbon cast-steel grit, to be used for blast cleaning and etchin...
Metallic Shot and Grit Mechanical Testing 2005 SAE SAE: J 445 JUL2005 This SAE Information Report is intended to provide users and producers of metallic shot and grit with general information on methods of mechanically testing metal shot in the labor...
Shot Peening, Automatic AMS 2430 M 2003 SAE SAE: AMS 2430 M Rev. 09/2003 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot. To induce residual...
Peening Media (ASR) Cast Steel Shot, Hard (45 to 52Hrc) AMS 2431 1C 2002 SAE SAE: AMS 2431/1C REV 02/2002 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Mechanical Methods for the Inducement of Residual Surface Compressive Stresses 2002 Ministry of Defence Defence Standard 03-21(Issue 3 DEF STAN 03-21/3 Publication Date 24 May 2002 REVISION NOTE This Standard has been revised in order to bring the technical methods and procedures into line with current practice and the format in...
AS9100 2001 SAE Aerospace SAE: AS900A, REV 08/2001 This document standardizes, to the greatest extent possible, quality management system requirements for the aerospace industry....
Test Strip Holder, and Gage for Shot Peening 2001 SAE SAE: J 442 Rev. December 2001 This SAE Standard defines requirements for equipment/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (test strip, holding fixture,...
Test Strip, Holder and Gage for Shot Peening 2001 SAE SAE: J 442 Rev Dec 2001 This SAE Standard defines requirments for equipmen/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (stst strip, holding fixture, a...
Shot Peening 2000 SAE SAE: J2441 2000-08 This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metalic shot, glass beads, or ceramic shot. The application is to induce resid...
Shot Peening 2000 SAE SAE: J 2441, Issued Aug 2000 This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Standard Specification for Brass, Copper, and Chromium-Plated Pipe Nipples 1999 ASTM ASTM Designation: B 687 - 99 1. Scope * 1.1 This specification establishes the requirements for brass and copper pipe nipples in standard pipe sizes from % to 8 in., inclusive, in standard lengths, and chromi...
Standard Test Method for Optical Emission Vacuum Spectrometric Analysis of Carbon and Low-Alloy Steel 1999 ASTM ASTM E 415 - 99 1.1 This test method covers the simultaneous determination of 20 alloying and residual elements in carbon and low-alloy steels in the concentration ranges shown (Note 1)....
Commercial Item Description Abrasive Materials; for Blasting 1999 U. S. Specification A-A-59316 Feb. 99; Superseding MIL-A-21380B July 65 SCOPE: This commercial item description (CID) covers newly manufactured mineral type abrasive materials used with pressure blasting equipment. The abrasives are generally used for...
Steel Grit, Shot and Cut Wire Shot; and Iron Grit and Shot-Blast Cleaning and Peening 1998 U.S. Military Specification MIL-S-851D Notice 4 18 Sept 1998 NOTICE OF CANCELLATION NOTICE OF CANCELLATION MIL-S-851D, dated 31 August 1990, is hereby canceled. Future acquisitions should be made using the current following documents:...
Standard Test Methods for Rockwell Hardness and Rockwell Superficial Hardness of Metallic Materials 1998 ASTM ASTM: E 18 - 98 SCOPE: 1.1 These test methods cover the determination of the Rockwell hardness and the Rockwell superficial hardness of metallic materials, including test methods for the verificat...
Residual Stress Measurement Xray 1998 SAE SAE: HSJ-0784: Notice of Cancellation Cancellation Notice...
Shot Peening of Metal Parts 1998 U. S. Specification MIL-S-13165C, Notice of Cancellation; Feb. 19, 1998 MIL-S-13165C, Dated 7 June 1989, and Amendment 1, dated 27 November 1991, are herby canceled. The preparing activity for this document has determined that AMS-S-13165, "Shot Peeni...
Test Strip, Holder and Gage for Shot Peening 1997 SAE SAE: J 442 Rev May 1997 This SAE Standard defines requirements for equipmen/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (test strip, holding fixture a...
Peening Media Cast Steel Shot, Hard (55 to 62Hrc) AMS 2431 2B 1997 SAE SAE: AMS 2431/2B Rev. 12/1997 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media (ASR) AMS 2431 1B 1997 SAE SAE: AMS 2431/1B, REV 12/01/1997 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Steel Grit, Shot, and Cut Wire Shot; and Iron Grit and Shot Blast Cleaning and Peening 1997 U. S. Specification MIL-S-851D, Notice of Cancellation, Superseding Notice 2 13/Dec/96 Mil-S-851D, Dated 31 Auguts 1990, is hereby cancelled, future acquisitions should be make usin the current following SAE documents: Type I cast steet grit should be replaced by ...
Abrasive Blasting 1997 U. S. Specification MIL-STD-1504B; Notice I MIL-STD-1504B, dated 8 June, 1989, and any subsequent revisions or change notices ae inactive for new design and shall be no longer used as a guidance reference for new design....
Sieve, Test 1997 U. S. Specification RR-S-366E, Notice of Cancellation; Notice 1 Federal Specification RR-S-366E, dated November 9, 1973 is hereby canceled. American Society for Testing and Materials (ASTM) Standards E-11 and E-323 may be used as replacement do...
Glass Beads, for Cleaning and Peening 1996 U. S. Specification MIL-G-9954A (Notice of Cancellation) 25 Apr 1996 MIL-G-9954, Rev A, dated 15 October 1987, is hereby canceled. Future acquisitions should be made using the current revision of AMS2431....
Steel Grit, Shot and Cut Wire Shot; And Iron Grit and Shot Blast Cleaning and Peening 1996 U. S. Specification MIL-S-851D Notice 2 (Superceding Notice 1 May 20, 1996) MIL-S-851D, dated May 20, 1996 is hereby reinstated and may be used for acquisition....
Aerospace Basic Quality System Standard 1996 SAE SAE: ARD9000 1. Scope: To assure customer satisfaction, aerospace industry manufacturers must produce world class quality products at the lowest possible cost. This document standardizes, to th...
Metallic Shot and Grit Mechanical Testing 1996 SAE SAE: J 445 Apr96 Forward - Shot testing machines differ in detail, but are alike in the fundamental principle that a sample of shot is subjected to repeated impacts on a target. The percentage of b...
Shot Peening, Computer Monitored 1996 SAE SAE: AMS 2432 B Revised 8/96 This specification establishes the engineering requirements for computer monitored peening of parts surfaces. This procedure has been used typically to induce, through cold workin...
Glass Bead Peening Procedures 1996 U. S. Specification MIL-STD-852 Notice of Cancellation no abstract...
Peening Media (AWRC)Hard (45 to 52 Hrc) AMS 2431 3B 1996 SAE SAE: AMS 2431/3B, REV 09/01/1991 The complete requirements for procuring the product shall consist of this document and the latest issue o the basic specification AMS 2431....
Steel Grit, Shot, and Cut Wire Shot; and Iron Grit and Shot-blast Cleaning and Peening 1996 U. S. Specification MIL-S-851D, 8 November 1996 (Reinstatement Letter: precedes notice 2) Reinstatement of MIL-S-851D via letter until formally reinstated. Gary Foy, Material Engineer, WR-ALC/LKJE, Robbins AFB, GA...
Peening Media Conditioned Stainless Steel Cut Wire Shot AMS 2431 4A 1996 SAE SAE: AMS 2431/4A, REV 099/01/1996 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification AMS 2431....
Peening Media Conditioned Carbon Steel Cut Wire Shot AMS 2431 3A 1996 SAE SAE: AMS 2431/3A, REV 09/01/1996 No abstract available...
Peening Media Cast Steel Shot, Hard (55 - 62 Hrc) AMS 2431 2A 1996 SAE SAE: AMS 2431/2A, REV 09/01/1996 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification AMS 2431....
Peening Media Cast Steel Shot, Regular (45-52 Hrc) AMS 2431 1A 1996 SAE SAE: AMS 2431/1A, REV 09/01/1996 The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431....
Peening Media General Requirements AMS 2431 A 1996 SAE SAE: AMS 2431A, REV 09/01/1996 This specification and its supplementary detail specifications cover the requirements for media to be used in controlled shop peening of metal parts. Reference to AMS 2431 with th...
Peening Media (AWCH) Conditioned Carbon Steel Cut Wire Shot, High Hardness (55 to 62Hrc) AMS 2431/8 1996 SAE SAE: AMS 2431/8, REV 09/01/1996 The complete requirements for procuring the product shall cinsist of this document and the latest issue of the basic specification AMS 2431...
Steel Grit, Shot, and Cut Wire Shot; and Iron Grit and Shot-blast Cleaning and Peening 1996 U. S. Specification MIL-S-851D Notice 1 20/May/1996 (cancellation) MIL-S-851D, dated 31 August 1990, is hereby canceled. Future acquisitions should be made using he current revision of AMS-2431...
Peening of Metal Parts 1995 U. S. Specification LPS 500 Shot and bead saturation peening or peen forming of aircraft parts using either manual, automatic, or computer controlled peening equipment....
Calibration System Requirements 1995 U. S. Specification MIL-STD-45662A (Notice of Cancellation; Apr 18, 1995) MIL-Std-45662A, dated 1 August 1988, is hereby cancelled. future acquisitions should refer to International Organization Measuring Equipment part 1...
Test Strip, Holder, and Gage for Shot Peening 1995 SAE SAE: J 442 Jan95 1. Scope - This SAE Standard defines requirements for equipment/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (test stip, holdin...
Peening of Metal Parts 1995 U. S. Specification NADEP/Jacksonville, FL. US Navy SUBJECT: Shot and bead saturation peening or peen forming of aircraft parts using either manual, automatic, or computer controlled peening equipment. PRUPOSE: This specification e...
Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel and in Iron, Nickel, & Cobalt Alloys 1994 ASTM ASTM E 1019 - 94 1.1 These test methods cover the determination of carbon, sulfur, nitrogen, and oxygen, in steel and in iron, nickel, and cobalt alloys having chemical compositions within the foll...
Standard Specification for Automated Controlled Shot Peening of Metallic Articles Prior to Nickel, Autocatalytic Nickel, or C 1994 ASTM ASTM: B 851 - 94 This specification covers the requirements for automated, controlled shot peening of metallic articles prior to lelctrolytic or autocatalytic deposition of nickel or chromium, or a...
Shot Peening AMS 2430 L 1993 SAE SAE: AMS 2430 L Rev. 07/1993 This specification covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot. To induce residual compressive ...
Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications. 1993 ASTM ASTM: E 29 - 93a The practice is intended to assist the various technical committees in the use of uniform methods of indicating the number of digits which are to be considered significant in speci...
Military Specification Abrasive Blasting Media Ship Hull blast Cleaning 1993 U. S. Specification MIL-A-22262B(SH) plus AMENDMENT 1 This specification covers nonmetallic abrasive materials used in the blast cleaning of metal surfaces and glass reinforced plastic surfaces, such as ships' hulls and tanks for remo...
Cast Shot and Grit Size Specifications for Peening and Cleaning 1993 SAE SAE: J 444 May93 This SAE recommended practice pertains to blast cleaning and shot peening and provided for standard cast shot and grit size numbers. For shot, this number corresponds with the ope...
Cut Wire Shot 1993 SAE SAE: J 441 Jun93 Superseding May 87, Revised 6-29-93 Cut wire shot shall be the product of carbon steel wire or stainless wire Type 302, 304 Condition B, spring Temper, cut into the form of cylinders with length approximately equal t...
Anodic Coatings for Aluminum and Aluminum Alloys 1993 U. S. Specification MIL-A-8625F This specification covers the requirements for six types and two classes of electrolytically formed anodic coatings on aluminum and aluminum alloys for non-architectural applicatio...
Shot Peening, Computer Monitored 1993 SAE SAE: AMS 2432 A Revised 1 Jan 1993 This specification establishes the engineering requirements for computer monitored peening of surfaces of parts. This procedure has been used typically to induce, through cold...
Standard Test Methods for Rockwell Hardness and Rockwell Superficial Hardness of Metallic Materials 1992 ASTM ASTM: E 18 These test methods cover the determination of the Rockwell hardness and the Rockwell superficial hardness of metallic materials, including methods for the verificaiton of machines ...
Military Specification Plastic Media, for Removal of Organic Coating 1992 U. S. Specification MIL-P-85891A plus AMENDMENT 1 This spedification covers six types of plastic media used for removal of organic coatings in an abrasive blast operation....
Nondestructive Testing Personnel Qualification and Certification 1991 U. S. Specification MIL-STD-410E, 25 January 1991 1. SCOPE 1.1 Purpose. This standard establishes the minimum requirements for the qualification and certification for personnel involved in the application of nondestructive inspec...
Abrasive Materials, for Blasting 1991 U. S. Specification MIL-A-21380B Notice 1 1991 MIL-A-21380G (1), dated 15 August 1979, has been reviewed and determined to be valid for use in acquisition....
Shot Peening of Metal Parts 1991 U. S. Specification MIL-S-13165C Amendment 1 27 November 1991 Page 16 Footnote 4/: Add to the second sentence for better clarification the following: "Unless otherwise specified on the drawing or in the contract, the peen...
SAE Manual on Shot Peening 1991 SAE SAE: HS-84 rev 3 Sep 1991 This manual on shot peening is intended to be a practical aid to engineers, designers and operators in the shop and points out some of the posibilities and some of the limitations ...
Low Carbon Steel Shot 1991 SAE SAE: J 2175 Jun91 1. Scope - This SAE Recommended Practice describes chemical analysis, hardness, microstructure, and physical characteristic requirements for low carbon cast steel shot to be used f...
Cast Shot And Grit Size Specifications For Peening And Cleaning 1991 SAE SAE: J 444 Aug84 Revised Proposed Draft Superseding J444 AUG 84 - This SAE Recommended Practice pertains to blast cleaning and shot peening and provides for standard cast shot and grit size numbers...
Standard Practices for Sampling Finished Lots of Metal Powders 1990 ASTM ASTM: B 215-90 Scope: 1.1 These practices cover two procedures for selecting representative samples of metal powders for subsequent testing: 1.1.1 Practice A - For powders in the process of bei...
Steel Grit, Shot and Cut Wire Shot, and Iron Grit and Shot Blast Cleaning and Peening - Amendment 1 1990 U. S. Specification MIL-S-851D Amendment 1 2.2.2:delete QQ-W-423 Wire, Steel, Corrosion Resisting 2.2: ADD Society of Automotive Engineers, Inc SAE J441 Cut wire shot, recommended practice...
Shot Peening, Computer Monitored 1990 SAE SAE: AMS 2432 This specification establishes the engineering requirements for computer monitored peening of surfaces of parts. To induce, through cold working, a surface layer that is residuall...
Shot Peening Of Aircraft Components 1990 U. S. Specification NAVAIRINST 4870.2, AIR-536A, June 4, 1990 Purpose is to establish and implement a policy for the application of shot peening in the manufacture and rework of aircraft components. This instruction applies to all peening op...
Cast Steel Shot 1990 SAE SAE: J 827 Mar90 This SAE Recommended Practice describes chemical analysis, hardness, microstructure and physical characteristic requirements for cast steel shot to be used for shot peening or blas...
Commercial Item Despciption Steel Grit 1989 U. S. Specification A-A-1041B THE GENERAL SERVICES ADMINISTRATION, HAS AUTHORIZED THE USE OF THIS COMMERCIAL ITEM DESCRIPTION IN FREFERENCE TO MILITARY SPECIFICATION MIL-S-851, TYPE I This commercial item desc...
Military Standard Abrasive Blasting 1989 U. S. Specification MIL-STD-1504B (Superseding MIL-STD-1504A Aug. 23, 1978) SCOPE: This standard covers the process and materials required for abrasive blasting of aircraft and missiles components....
Shot Peening of Metal Parts 1989 U. S. Specification MIL-S-13165C This specification is approved for use by all Departments and Agencies of the Department of Defense. 7-June-1989 superseding MIL-S-13165B 31-Dec-1966 ...
Steel Grit, Shot, And Cut Wire Shot; And Iron Grit And Shot-blast Cleaning And Peening 1989 U. S. Specification MIL-S-851D 21 April 1989 This specification covers cast iron or hardened cast steel grit and shot for blast cleaning of castings, forgings, ship hulls and decks, or other parts prior to use for the removal...
Cast Steel Grit, Proposed Specification 1989 SAE SAE: J 1993 This SAE recommended practice describes the chemical composition, and physical characteristic requirements for high carbon cast steel grit, to be used for blast cleaning and etchin...
Glass Bead Peening Procedures 1988 US Government MIL-STD-852 Notice 1 US Government MIL-STD-852 Notice 1 MIL-STD-852, dated 21 Sep 1965, has been reviewed and determined to be valid for use in acquisition. ...
Calibration Systems Requirements 1988 U.S. Specification MIL-STD-45662A This military standard contains requirements for the establishment and maintenance of a calibration ayatem used to control the accuracy of measuring and test equipment (M&TE) and m...
Steel Shot - Commercial Item Description 1988 U. S. Specification A-A-1042B This commercial item description covers hardened steel shot for general blasting and peening purposes. (The General Services Administration has authorized the use of this commercia...
Commercial Item Description Steel Shot 1989 U. S. Specification A-A-1042B THE GENERAL SERVICES ADMINISTRATION HAS AUTHORIZED THE USE OF THIS COMMERCIAL ITEM DESCRIPTION IN LIEU OF MILITARY SPECIFICATION MIL-S-851C. This commercial item description cover...
Calibration Systems Requirements 1988 U. S. Specification MIL-STD 45662A 1 August 1988 This military standard contains requirements for the establishment and maintenance of a calibration system used to control the accuracy of measuring and test equipme...
Size Classification And Characteristics Of Glass Beads For Peening 1988 SAE SAE: J 1173 Sep88 This specification covers the characteristics of glass beads used for peening, and provides for standard glass bead size numbers. The glass bead classification number is the appro...
Shot Peening AMS 2430 K 1988 SAE SAE: AMS 2430 K Rev. 04/1988 This specification covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, and ceramic shot. To induce residual compressiv...
Plastic Media, For Removal Of Organic Coatings 1988 U. S. Specification MIL-P-85891(AS) 6 May 1988 This specification covers five types of plastic media used for removal of organic coatings in an abrasive blast operation: (I) Polyester (Thermoset); (II) Urea Formaldehyde (Therm...
Peening Media Glass Shot AMS 2431 6 1988 SAE SAE: AMS 2431/6, REV 04/l0/1988 This specification, in conjunction with the general requirements covered in AMS 2431 established the requirements for glass shot to be used for peening of metal parts. Descriptors...
Peening Media General Requirements AMS 2431 1988 SAE SAE: AMS 2431, REV 04/l/1988 This specification establishes general requirements for the media to be used in controlled shot peening of metal parts. Reference to AMS 2431 with appropriate slash number on a p...
Peening Media Conditioned Stainless Steel Cut Wire Shot AMS 2431 4 1988 SAE SAE: AMS 2431/4, REV 04/01/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for conditioned stainless steel cut wire shot to be used for peen...
Peening Media Conditioned Carbon Steel Cut Wire Shot AMS 2431 3 1988 SAE SAE: AMS 2431/3, REV 04/01/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for conditioned carbon steel cut wire shot to be used for peening...
Peening Media Ceramic Shot AMS 2431 7 1988 SAE SAE: AMS 2431/7, REV 04/01/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for ceramic shot, for peening of metal parts. Descriptors: Quali...
Peening Media Cast Steel Shot, Hard (55 - 62 Hrc) AMS 2431 2 1988 SAE SAE: AMS 2431/2, REV 04/0l/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for hard cast steel shot to be used for peening of metal parts. ...
Peening Media Cast Steel Shot, Regular (45 - 52 Hrc) AMS 2431 1 1988 SAE SAE: AMS 2431/1, REV 04/0l/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for regular cast steel shot to be used for peening of metal parts...
Peening Media Case Hardened Steel Peening Balls AMS 2431 5 1988 SAE SAE: AMS 2431/5, REV 04/01/1988 This specification, in conjunction with the general requirements covered in AMS 2431, establishes the requirements for peening balls to be used for peening of metal parts. Descrip...
Aluminum Alloy Sheet And Plate 1.0mg-0.60si-0.28cu-0.20cr(6061;-t6 Sht,-t651 Plate) Solution And Precipitation Heat Treated 1988 SAE SAE: AMS 4027K This specificationcovers an aluminum alloy in the form of sheet and plate. Primarily applicable for parts where strength is required and limited formability is acceptable....
Balls, Bearing, Ferrous and Non-Ferrous (for use in Bearings, Valves and Bearing Applications) General Specification for 1987 U. S. Specification MIL-B-1083D 16 OCT 87 This specification is approved for use by all departments and agencies of the Department of Defense. This specification covers requirements for ferrous and non-ferrous inch balls....
Standard Specification For Wire-cloth Sieves For Testing Purposes 1987 ASTM ASTM: E 11-87 This specification covers the design and construction of sieves wherein a screening medium of woven wire cloth is mounted in a frame for use for precision testing in the classifica...
Peening Of Metal Parts Local Process Specification (lps/jx 341-149-87) 1987 U. S. Specification LPS/JX 341-149-87 This specification establishes the materials, equipment, procedures and requirements applicable to metallic shot and glass bead saturation peening and peen forming of aircraft part...
Japan's Launch Vehicle Program Update 1987 Tadakawa, Tsuguo SAE: 871340 National Space Development Agency of Japan, NASDA, as an implementing agency in Japan for space applications missions, has successfully developed N series program, so called N-I an...
Cut Wire Shot 1987 SAE SAE: J 441 May87 Cut wire shot shall be the product of carbon steel wire or stainless wire Type 302, 304 Condition B, spring Temper, cut into the form of cylinders with length approximately equal t...
Case History Of Dry Paint Stripping 1987 Hammond, D. SAE: 870754 The purpose of this paper is to present an overview of the use of the dry paint stripping process in the aircraft industry. It spotlights the major influencing factors of three cu...
Manufacturing Sequence for Fabrication of High-Strength Steel Parts 1984 SAE SAE: ARP 1631 This document establishes the requirements for the sequencing of processes relating to parts fabricated from 300M ro 4340 modifies steel heat treated to, or to be heat treated to 2...
Procedures for Using Standard Shot Peening Test 1984 SAE SAE: J 443 Jan84 This SAE Recommended Practice provides uniform procedure for using the standard shot peening test strips in SAE Standard J442, Test Strip, Holder and Gage for Shot Peening. Descri...
Military Specification Peening Of Metals, Mil-p-81985(as) Amendment 1 1984 U. S. Specification MIL-P-81985(AS) Amendment 1 This specification covers procedures and requirements for dry peening the surfaces of metals by impingement of metallic shot or glass beads for the purpose of increasing the fatigu...
Metallic Shot And Grit Mechanical Testing 1984 SAE SAE: J 445 Aug84 This report is intended to provide users and producers of metallic shot and grit with general information on methods of mechanically testing metal abrasives in the laboratory. Des...
Aluminum Alloy 2024, Plate and Sheet 1983 U. S. Specification QQ-A-250/4E INTERIM AMENDMENT (superseding amendment-1, Oct 22, 1974) The interim amendment was developed by the Naval Air Systems Command, Department of the Navy, Washington, DC 20361, based upon current available technical information. It is recom...
Shot Peening AMS 2430 J 1982 SAE SAE: AMS 2430 J Rev. 01/1982 This specification covers the engineering requirements for peening surfaces of parts by impingement of metallic shot or glass beads....
Federal Specification Sheet Aluminum Alloy 6061, Plate And Sheet 1982 U. S. Specification QQ-A-250/11F (Superseding QQ-A-250/11E Aug. 27, 1971) This specification covers the specific requirements for aluminum alloy 6061 plate and sheet....
Surface Rolling and Other Methods for Mechanical Prestressing of Metals - SAE J811 AUG81 1981 SAE SAE: J 811 Aug81 1.1 INTRODUCTION: The word "prestressing" implies that a stress is applied prior to service. for the pruposes of this discussion this is a true but insufficient, definition. It m...
Commercial Item Description Grain, Abrasive (Soft Blasting) 1981 U. S. Specification A-A-1722 THE GENERAL SERVICES ADMINISTRATION HAS AUTHORIZED THE USE OF THIS COMMERCIAL ITEM DESCRIPTION IN PREFERENCE TO MILITARY SPECIFICATION MIL-G-5634 This commercial item description ...
Magnesium Alloys, Anodic Treatment Of 1981 U. S. Specification MIL-M-45202C This specification covers the requirements for equipment, materials and procedures to be used in anodic treatments of magnesium base alloys for the purpose of increasing their corr...
Glass Beads: For Cleaning And Peening, amend 2 1980 U. S. Specification MIL-G-9954A, Amend. 2 This specification covers glass beads to be used with pressure/suction type blasting equipment....
Calibration Systems Requirements 1980 U. S. Specification MIL-STD-45662 (Superseding MIL-C-45662A Feb. 9, 1962) 10 June 1980 This standard provides for the establishment and maintenance of a calibration system to control the accuracy of the measuring and test equipment used to assure that s...
Abrasive Materials, for Blasting 1979 U. S. Specification MIL-A-21380B Amendment 1 1979 This amendment forms a part of Military Specification MIL-A-21380B, dated 15 July 1965, and is approved for use by all Departments and Agencies of the Department of Defense....
Test Strip, Holder and Gage for Shot Peening 1979 SAE SAE: J 442 Aug79 This SAE Standard is supplemental by an SAE Recommended Practice, Procedures for Using Standard Shot Peening Test Strip, SAE J443. Outline of Method of Control--The control of a...
Steel Grit, Shot, And Cut Wire Shot; And Iron Grit And Shot-blast Cleaning And Peening 1979 U. S. Specification MIL-S-851C Amendment This amendment forms a part of Military Specification MIL-S-851C, 30 May 72....
Aluminum and Aluminum Alloy Plate and Sheet: General Specifications for 1978 U. S. Specification QQ-A-250F (Superseding QQ-A-250E Oct. 19, 1970) This specifiction was approved by the commissioner, Federal Supply Service, General Services Administration, for the use of all federa agencies. The specification covers the gene...
Federal Specification Sieve Test 1978 U. S. Specification RR-S-366E This specification covers woven-wire-cloth sieves, and round-hole and square-hole, perforated-plate sieves intended for general use in the classification of materials according to ...
Test Strip, Holder and Gage for Shot Peening 1977 SAE SAE: J 442 Rev 1977 This SAE standard is supplimented by an SAE Recommended Practice, Procedures for Using Standard Shot Peening Test Strip, SAE J443. ...
Size Classification And Characteristics Of Ceramic Shot For Peening 1977 SAE SAE: J 1830 May87 This specification covers characteristics for chemistry, microstructure, density, hardness, size, shape and appearance of zirconium oxide based ceramic shot, suitable for peening s...
Technical Report on Fatigue Properties - SAE J1099 1975 SAE SAE: J 1099 1.0 Scope 1.1 Pertinent information to provide design guidance in avoiding fatigue failures is outlined in this SAE Information Report. Of necessity, it is brief, but it does prov...
Aluminum Alloy 2024, Plate and Sheet 1974 U. S. Specification QQ-A-250/4E AMENDMENT-1 This amendment, which forms part of Federal Specification QQ-A-250/4E, dated January 18, 1971, was approved by Commissioner, Federal Supply Service, General Services Administration...
Chromium Plating (Electrdeposited) 1974 U. S. Specification QQ-C-320B Amend4 4/87 Amend2 11/84 Abstract: QQ-C-320B AMENDMENT 4 10 April 1987 SUPERSEDING AMENDMENT 3 7 June 1985 This amendment, which forms a part of QQ-C-320B dated 17 June 1974, was approved by the Commission...
Peening of Metals 1974 U. S. Specification MIL-P-81985 (AS) This specification has been approved by the Naval Air Systems Command, Department of the Navy. This specification covers procedures and requirements for dry peening the surface...
Federal Specification Sieve, Test 1973 U. S. Specification RR-S-366D This specification covers woven-wire-cloth sieves, and round-hole and square-hole, perforated-plate sieves intended for general use in the classification of materials according to ...
Shot Peening 1972 SAE SAE: AMS 2430 H Rev. 05/1972 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Steel Grit, Shot and Cut Wire Shot; and Iron Grit and Shot - Blast Cleaning and Peening 1972 U. S. Specification MIL-S-851C (Superseding MIL-S-851B 26 Sept 55) This specification is approved for use by all Departments and Agencies of the Department of Defense. This specification covers cast iron or hardened cast steel grit and shot for b...
Rotary Flap Peening Of Metal Parts 1972 U. S. Specification MIL-R-81841(AS) This specification covers procedures and requirements for peening of metal parts with portable bonded-shot rotary flap wheels....
Military Specification Wheels, Peening, Rotary Flap 1972 U. S. Specification MIL-W-81840(AS) This specification covers rotary flap wheels used with portable equipment for peening of metal parts....
Aluminum Alloy 2024, Plate and Sheet 1971 U. S. Specification QQ-A-250/4E (Superseding QQ-A-250/4D Mar. 17, 1967) The specification covers the specific requirements for aluminum alloy 2024 plate and sheet; the general requirements are covered in QQ-A-250....
Surfaces Treatments And Inorganic Coatings For Metal Surfaces Of Weapons Systems 1971 U. S. Specification MIL-S-5002C This specification covers the requirements for cleaning, surface treatments and inorganic coatings for metallic surfaces of weapons systems parts....
Shot Peening AMS 2430 G 1971 SAE SAE: AMS 2430 G, Rev. 11/1971 This specification covers the engineering requirements for peening surfaces of parts by impingement of metallic shot or glass beads....
Military Specification Grain, Abrasive, Soft for Carbon Removal 1970 U. S. Specification MIL-G-5634C plus AMENDMENT 2 and 3 This specification covers soft abrasive grains to be used as abrasive blasting material for the removal of carbon from metal surfaces, and cleaning of operating jet engines....
Shot Peening 1969 SAE SAE: AMS 2430 F Rev. 05/1969 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Manual On Blast Cleaning - Sae J792a 1968 SAE SAE: J 792a This manual on blast cleaning is a companion to the SAE Manual on Shot peening. It is intended to help engineers, management, and shop personnel to increase their knowledge of the...
Shot Peening 1966 SAE SAE: AMS 2430 E Rev. 09-1966 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Shot Peening Of Metal Parts 1966 U. S. Specification MIL-S-13165B This specification covers procedure requirements for shot peening of metal parts, to induce residual compressive stresses in specified surfaces, for the purpose of increasing the f...
Glass Beads: For Cleaning And Peening 1966 U. S. Specification MIL-G-9954A This specification covers glass beads to be used with pressure/suction type blasting equipment....
Military Specification Abrasive Material for Blasting 1965 U. S. Specification MIL-A-21380B This specification covers mineral type abrasives used with pressure blasting equipment to descale, clean, and finish metallic parts....
Glass Bead Peening Procedures 1965 U. S. Specification MIL-STD-852 This standard establishes minimum requirements and procedures for glass bead peening of ferrous and non-ferrous parts which are subjected to repeated applications of stress such as...
Shot Peening 1963 SAE SAE: AMS 2430 D Rev. 07/1963 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Sampling Procedures And Tables For Inspection By Attributes 1963 U. S. Specification MIL-STD-105D This publication establishes sampling plans and procedures for inspection by attributes. When specified by the responsible authority, this publication shall be referenced in the s...
Inspection System Requirements 1963 U. S. Specification MIL-I-45208A This specification establishes requirements for contractors' inspection systems. These requirements pertain to the inspections and tests necessary to substantiate product conforma...
Surface Rolling And Other Methods For Mechanical Prestressing Of Metals 1962 SAE SAE: J 811 Jun62 With the need for more efficient use of metals, consideration of mechanical prestressing during the design phase seems obvious, for the vast majority of fractures are caused by met...
Shot Peening 1961 SAE SAE: AMS 2430 C Rev. 07/1961 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Test Strip, Holder And Gage For Shot Peening - Sae J442 1961 SAE SAE: J 442 Rev. June 1961 This SAE Standard is supplemented by an SAE Recommended Practice, Procedures for Using Standard Shot Peening Test Strip, SAE J443. The control of a peening machine operation is pr...
Procedures For Using Standard Shot Peening Test Strip 1961 SAE SAE: J 443 Jun61 This SAE Recommended Practice provides uniform procedure for using the standard shot peening test strips in SAE Standard J442, Test Strip, Holder and Gage for Shot Peening. Descri...
Shot Peening of Ferrous Metal Parts 1956 U. S. Specification MIL-S-13165A This specification has been approved by the Department of Defense and is mandatory for use by the Departments of the Army, the Navy, and the Air Force. This specification covers s...
Manual On Blast Cleaning 1953 SAE SAE: J 792 This manual on blast cleaning is a companion to the one published on shotpeening. It is intended to help engineers, management, and shop personnel to increase their knowledge of t...
Procedures for Using Standard Shot-Peening Test Strip 1952 SAE SAE: J 443 The test strip A is used for arc height up to 0.024 A (See arc-height designation given in SAE Standard Test Strip, Holder, and Gage for Shot Peening. ) For greater degrees of peen...
Test Strip, Holder, and Gage for Shot Peening 1952 SAE SAE: J 442 Jan52 Outline of Method of Control- The control of a peening machine operation is primarily a matter of the control of the properties of a blast of shot in its relation to the work bein...
Shot Peening 1951 SAE SAE: AMS 2430 A Rev. 10/1951 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot....
Metal Grit And Shot For Blast Cleaning And Peening 1950 U. S. Specification MIL-M-851-A This specification covers chilled or hardened iron or steel grit and shot for blast cleaning of sand, slag, rust and marine incrustations from castings, forgings, ship hulls and de...
Shot Peening 1948 SAE SAE: AMS 2430 B Rev. 11/1954 This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot. ...
Shot Peening AMS 2430 1948 SAE SAE: AMS 2430, Issued 09/01/1948 To impose compressive stresses on specified surface layers of metallic parts, primarily for increasing fatigue strength but may be used for other purposes such as testing for bond ...
Shot Peening of Metals, General Specification For 1944 U. S. Specification AXS-1272 (Rev. 1) Ordinance Department U. S. Army Tentative Specification 31 August, 1944 (ed. This is the predecesor to MIL-S-13165, Shot Peening of Metals)...