Abstract:  
A sample of new CW-41 Cut Steel Wire Shot, C-41 Cut Steel Wire Shot operating mix, CW-41 Cut Steel Wire Shot separator discharge and an Almen C Test Strip peened in the production machine, were received from Rockwell Standard Corporation in New Castle, Pennsylvania. The information obtained from the above samples was to be used in conjunction with information derived from Ervin Test Machine results to determine a size of cast steel shot that would be more economical than the CW-41 Cut Steel Wire Shot presently used for peening leaf springs.