Abstract:  
Paper consititutes a sumary of investigation conducted by the authors and encompasses the experimental apparatus design, the heating and quenching of test specimens, the recording of the time-temperature history of the plate during cooling, and the experimental measuring of the residual stresses which have been induced in the plate by the quenching.