Material And Processing Effects On Fatigue Performance Of Leaf Springs

Author:  Landgraf, R.W. and Francis, R.C.
Source:  Conf: Congress and Expos.,Mar.'79 (Book)
Doc ID:  1979017
Year of Publication:  1979
Abstract:  
Procedures are developed for assessing the influence of various material and processing factors on the fatigue performance of leaf springs. Cyclic material properties, determined from smooth axial specimens of spring steel, are used to determine the level and cyclic stability of residual stresses resulting from mechanical processing as well as the amount of permanent deformation associated with presetting operations. A damage parameter, incorporating material properties, residual stress effects and applied stressing conditions, is used to predict failure location, i.e., surface or subsurface, and lifetime as a function of processing sequence. Predictions are found to be in good agreement with experimental bending results. Descriptors: Shot peening; Springs; Residual stresses; Ferrous metals; Fatigue