Effects Of Multiple Shot Peening/cadmium Plating On High Strength Steel
Author: Kohls, John and Stross, William
Source: Tech. Rep: AFWAL-TR-80-4005
Doc ID: 1980003
Year of Publication: 1980
Abstract:
The effect of multiple shot peening and Cd plating operations on a high-strength steel alloy used in landing gear applications is studied. The basis for determining this effect was fatigue and stress corrosion tests in a high humidity environment.
Descriptors: High strength steels-- Structural hardening; Cadmium plating; Shot peening; Stress corrosion; Fatigue strength; Strain hardening; Landing gear