High Sag Resistance Spring Wire For Automotive Suspension

Author:  Murai,Teruyuki,Takamuku,Seizo, etc.
Source:  SAE: 850059
Doc ID:  1985033
Year of Publication:  1985
Abstract:  
In recent years, efforts have been undertaken to increase the stress load on spring materials and to decrease wire diameter in order to reduce weight. However, progress has been slow due to the resulting increase in spring sag. This report describes the characteristics of steel wire subjected to a new strain method. After quenching and tempering, while the wire is still warm, strain is imposed on the wire to improve its sag resistance. Results show that sagging in springs made of this wire is approximately one half that of springs made of conventionally quenched and tempered wire of the same strength. Moreover, strain-imposed wire can be quenched and tempered to a lower strength than, yet have the same sag resistance as, extremely high strength conventional wire. As a result, problems encountered when high strength material is used to improve sag resistance--such as damaged cutting tools and decreased shot peening effect--can be avoided. After practical application, the fatigue life of this wire has been confirmed to be sufficient for commercial use. Descriptors: Springs; Steels; Stresses; Suspension systems; Tensile strength; Wire


Download PDF