Automation of Post-fabrication Processes

Author:  Fuller, P.A.
Source:  Elsevier Appl.Sci.Publ. Essex UK '86 (Book)
Doc ID:  1986079
Year of Publication:  1986
Abstract:  
Shot peening is an important post-fabrication process at Alvis. The methods used for shot peening A1 armour welded assemblies (A1-An--Mg alloy) have not previously attracted significant attention in the area of improved processing techniques. Alvis has commenced a work programme using micro-processor based controls and robotics to provide for a productionised automated system. The requirements necessary to create a facility for the automated shot peening of A1 armour plate assemblies are outlined. Descriptors: Armor-- Structural hardening; Aluminum base alloys-- Structural hardening; Shot peening-- Automation; Industrial robots; Painting