Peening Improves Fatigue Life

Author:  Welsch, Win
Source:  Welding Design & Fabrication, Sept. '90, p.38
Doc ID:  1990050
Year of Publication:  1990
Abstract:  
Fabricators in the aerospace and automotive industries use shotpeening to extend fatigue life of welded joints. Another benefit: resistance to stress-corrosion cracking.