Surface Treating Method for Steel Pipe Joint Text in Japanese
Author: Atsumi Takuya
Source: Japanese Patent JP6099354
Doc ID: 1994070
Year of Publication: 1994
Abstract:
PURPOSE:To improve seal performance by applying shot peening to at least one of metal to metal seal parts, and adjusting a surface roughness degree after the shot peening to the metal to metal seal parts, so as to reduce unevenness of a limit value of the seal performance. CONSTITUTION:In a steel pipe joint 2 of containing 2% or less Cr by weight ratio and also having a metal to metal seal part 4, shot peening is applied to at least one of the metal to metal seal parts 4. Now when assumed x (mum) for surface mean roughness and y (mum) for maximum roughness after the shot peening of the metal to metal seal part 4, surface roughness is adjusted so as to satisfy
a relation where 1.50<=x<=5.0, 10<=y<=30.
|
|---|