Abstract:  
Unfortunatly, we don't know who wrote this article and therefore cannot give credit for this pratical and enlightening series. However, we can thank Ken Dykstra of Precision Automation Inc. for submitting it to us for publication. Impact cleaning, commonly called grit blasting or sandblasting, is a process of bombarding a work surface with small particles traveling at high speeds.