Centrifugal Wheel Peening Principals - Part 2 of a 3 part series

Author:  Eugene A. Tarabek
Source:  ABC, Vol 1/ No 2, Spring 1996
Doc ID:  1996169
Year of Publication:  1996
Abstract:  
Setting the Blast Pattern Before attempting to set a blast pattern all the integral parts, including the blades/vanes, impeller and control cage/impeller case, should be replaced.