Effective Use of Steel Shot and Grit for Blast Cleaning

Author:  E. A. Borch, Ervin Industries, Inc.
Source:  ABC, Vol 4/ No 4, Fall 1999
Doc ID:  1999109
Year of Publication:  1999
Abstract:  
Essential for an effective and cost efficient blast cleaning operation is a solid, basic understanding of the charateristics of cast steel blast cleaning abrasives, their selections and use, as well as knowledge of blast cleaning equipment, its maintenance, and key process control features.