Centrifugal Wheel Peening Principles - Part 2 of a 5 part series

Author:  Eugene A. Tarabek
Source:  ABC, Vol 4/ No 3, Summer 1999
Doc ID:  1999115
Year of Publication:  1999
Abstract:  
Part two of a five part series by Eugene Tarabek Eugene Tarabek is president of Tarabek, Inc., a consulting firm that provides tech support for blast cleaning and shot peening equipment. Setting the Blast Pattern: Before attempting to set a blast pattern all the integral parts, including the blades/vanes, impeller and control cage/impeller case, should be replaced.