The Critical Operations of Shot Peening.

Author:  Caterpillar Inc. CAT 1E 2054 Spec
Source:  Caterpillar Inc
Doc ID:  2000001
Year of Publication:  2000
Abstract:  
This specification shall be applied to highly stressed parts, such as axle shafts, connecting rods, springs, etc., on which shot peening is required for increased fatigue resistance