Simple Fixturing Enhances Work Car's Versatiltiy
Author: Herb Tobben, Manager
Source: ABC, Vol 5/ No3, Summer 2000
Doc ID: 2000053
Year of Publication: 2000
Abstract:
Sample Processing Laboratory
Zero Products Div., Clemco Industries Corp.
Reprinted with permission
An aircraft component manufacturer was using an old blast room and non-recyclable abrasives to etch aluminum alloy parts prior to coating. The company hoped to get its employees out of the blast environment entirely, possibly through automation.