Method for Forming a Metallic Coat by Impacting Metallic Particles on a Workpiece
Author: Yoshio Miyasaka, Kasugai (JP)
Source: US Patent 6,291,012 B1
Doc ID: 2001016
Year of Publication: 2001
Abstract:
ABSTRACT
Method for forming metallic coat where, the surface of workpiece is partly covered with a masking material having a predetermined pattern, and metallic powders are ejected to the surface at the ejection velocity of 80 m/sec or higher or at the ejection pressure of 0.3 Mpa or higher by utilizing an ejection apparatus such as blast work apparatus, in order to easily attain the metallic coat having high adhesion strength without washing process, nor heat process by a relatively simple facility.