Achieving and Maintaining Required Roll Ra and PC via Steel Grit Blasting
Author: E.A. Borch
Source: ABC, Vol 6/ No 4, Fall 2001
Doc ID: 2001136
Year of Publication: 2001
Abstract:
Reprinted with permission from Ervin Industries
Steel grit blasting can produce virtually any required roll profile but only when the relationship of grit work mix size distribution to Ra and PC is fully understood, and rigid operating disciplines to control correct size distribution are practiced. Described are: work mix size and profile relationships, control measures needed.