Cut-Wire Type Ferrous Shot for Blasting and a Process of Using a Cut-Wire Type Ferrous Shot for Blasting
Author: T Watanabe; S Murai; N Murai; Y Watanabe; Hattori
Source: US Patent 6,394,881 B1
Doc ID: 2002080
Year of Publication: 2002
Abstract:
The present invention discloses a cut wire method of producing a ferrous shot and a cut-wire type ferrous shot for shot-blasting having a hardness of Hv 200 to 300 and a low work hardening ability. Further, the present invention describes a process of using a cut-wire type ferrous shots, comprising preparing the cut-wire type ferrous shots and a ferrous object and projecting the shots to the ferrous object to remove foreign material from the ferrous object.