Cast Steel Shot and Grit - The Miracle Workers of Blast Cleaning, Profiling, Peening
Author: Ervin Industries
Source: ABC, Vol 7/ No 3, Summer 2003
Doc ID: 2002125
Year of Publication: 2002
Abstract:
Part 3 of a 5 part series
Reprinted with permission from Ervin Industries
Technical Bulletin October, 1995
In Part Two, the only miracle we asked of Cast Steel Shot/Grit and the abrasive blast equipment was to remove surface contaminants from the workpiece, and we explained how selection of abrasive size affects the effectiveness and efficiency of the operation. Now, in Part Three, we ask for two miracles: Remove the contaminant; AND provide a controlled anchor pattern profile that will assure optimum adherence and durability when bonding, painting, or coating the workpiece.