Cold Working Cold Metal - A Hot Topic
Author: Herb Tobben, Manager
Source: ABC, Vol 7/ No 2, Spring 2002
Doc ID: 2002130
Year of Publication: 2002
Abstract:
Sample Processing Lab
ZERO Products Div., Clemco Industries Corp.
Reprinted with permission
The Problem:
A cryogenics container manufacturer needed to clean and finish the exterior surfaces of stainless steel tanks. At first glance, the containers resemble beer kegs, but with more fittings, plus a beefier base and lifting attachments. They range in size from 16 to 32 inches tall and up to 16 inches in diameter.
| Download PDF |
|---|