Method and Apparatus for Improveing Media Flow US Patent 7,291,058 B2
Author: Jack Champaigne
Source: US Patent 7,291,058 B2
Doc ID: 2007032
Year of Publication: 2007
Abstract:
ABSTRACT
The flow of media in shot peening, blast cleaning, and similar equipment is improved by applying a time varying magnetic field to the media to thereby degauss the media, allowing the media to flow through equipment without clogging and clumping due to magnetic attraction between the media.