Methods for Improving Fatigue Performance of Implants with Osteointegrating Coatings
Author: Hai H. Trieu, Frank Bono
Source: US Patent 2008/0221681A1
Doc ID: 2008130
Year of Publication: 2008
Abstract:
ABSTRACT
A method which may be used for introducing a residual compressive stress into a body portion of an implantable device configured for implantation in a patient. The body portion may include an outer surface. The method also may include texturing the outer surface of the implantable device to increase a roughness of the outer surface. The outer surface may be coated with an osteointegrating material to increase osteointegration.