Shot Peening
Author: SAE
Source: SAE: AMS 2430 C Rev. 07/1961
Doc ID: 1961021
Year of Publication: 1961
Abstract:
This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
|
|---|
| For more information: http://www.sae.org |
|---|