Glass Composition for Beads
Author: C.E. Searight; E.M. Alexander
Source: US Patent 3,071,480
Doc ID: 1963018
Year of Publication: 1963
Abstract:
This invention relates to an improved glass composition and, more particularly, to a glass composition suitable for the manufacture of solid spherical glass beads.