Quick-Drying Scouring Composition
Author: Monick, John Alexander
Source: US Patent 3,607,161
Doc ID: 1971011
Year of Publication: 1971
Abstract:
A scouring composition comprising a cationic surface active compound and a water-soluable abrasive which leaves a surface which has been cleaned dry, shiny an dfree from gritty residue film.