Size Classification And Characteristics Of Ceramic Shot For Peening
Author: SAE
Source: SAE: J 1830 May87
Doc ID: 1977007
Year of Publication: 1977
Abstract:
This specification covers characteristics for chemistry, microstructure, density, hardness, size, shape and appearance of zirconium oxide based ceramic shot, suitable for peening surfaces of parts by impingement. This specification includes the nominal chemistry of zirconium oxide based ceramic shot and the amount of free iron particles.
Descriptors: Shot; Ceramics--shot: Zirconium oxide; Physical properties--ceramic shot
|
|---|