Descaling Bent Rod With Separated Cleaning Particles
Author: Joseph Johannes, Maria Annegarn
Source: US Patent 4,004,374
Doc ID: 1977066
Year of Publication: 1977
Abstract:
A method of descaling a rod comprises forming at least one bend in the rod and rotating the bent portion in an approximately circular path while maintaining it in a space having a distribution of separated cleaning particles therin in a suspended relationship relative thereto. The rotating bent portion strikes the distributed particles and is cleaned thereby.