Method of Abrading or Having a Restricted Passage Surface
Author: Perry, Kenneth E.
Source: US Patent 4,087,943
Doc ID: 1978013
Year of Publication: 1978
Abstract:
A flowable abrasive composition comprising a poluboronorgano silicon compound and dispersed abrasive granules, said composition being modified with a gel formed from a metallic soap(8-22 carbon atoms) and a hydrocarbon oil. The composition is expecially useful for honing, abrading, deburring or polishing surfaces, expecially metallic surfaces.