Magnesium Alloys, Anodic Treatment Of
Author: U. S. Specification
Source: MIL-M-45202C
Doc ID: 1981086
Year of Publication: 1981
Abstract:
This specification covers the requirements for equipment, materials and procedures to be used in anodic treatments of magnesium base alloys for the purpose of increasing their corrosion resistance or producing surfaces suitable for the application of a protective organic finish.
|
|---|