Metallic Shot And Grit Mechanical Testing
Author: SAE
Source: SAE: J 445 Aug84
Doc ID: 1984046
Year of Publication: 1984
Abstract:
This report is intended to provide users and producers of metallic shot and grit with general information on methods of mechanically testing metal abrasives in the laboratory.
Descriptors: Grit; Shot peening
|
|---|