Peening of Metals MIL-P-81985 Amendment 1
Author: US Government Spec
Source: US Government Spec
Doc ID: 1984139
Year of Publication: 1984
Abstract:
This amendment forms a part of Military Specification MIL-P-81985(AS) dated 18 October 1974, and is approved for use by the Naval Air Systems Command, Department of the Navy and is available for use by all Departments and Agencies of the Department of Defense