Steel Grit, Shot, And Cut Wire Shot; And Iron Grit And Shot-blast Cleaning And Peening
Author: U. S. Specification
Source: MIL-S-851D 21 April 1989
Doc ID: 1989019
Year of Publication: 1989
Abstract:
This specification covers cast iron or hardened cast steel grit and shot for blast cleaning of castings, forgings, ship hulls and decks, or other parts prior to use for the removal of sand, slag, rust, and marine incrustations; and also cast iron or hardened cast steel shot, or cut steel wire shot for peening the surface of metals.
| Download PDF |
|---|