Cast Steel Shot
Author: SAE
Source: SAE: J 827 Mar90
Doc ID: 1990009
Year of Publication: 1990
Abstract:
This SAE Recommended Practice describes chemical analysis, hardness, microstructure and physical characteristic requirements for cast steel shot to be used for shot peening or blast cleaning operations.
|
|---|