Low Carbon Steel Shot
Author: SAE
Source: SAE: J 2175 Jun91
Doc ID: 1991011
Year of Publication: 1991
Abstract:
1. Scope - This SAE Recommended Practice describes chemical analysis, hardness, microstructure, and physical characteristic requirements for low carbon cast steel shot to be used for shot peening of blast cleaning operations.
|
|---|