SAE Manual on Shot Peening
Author: SAE
Source: SAE: HS-84 rev 3 Sep 1991
Doc ID: 1991019
Year of Publication: 1991
Abstract:
This manual on shot peening is intended to be a practical aid to engineers, designers and operators in the shop and points out some of the posibilities and some of the limitations of the process.
|
|---|