Military Specification Plastic Media, for Removal of Organic Coating
Author: U. S. Specification
Source: MIL-P-85891A plus AMENDMENT 1
Doc ID: 1992038
Year of Publication: 1992
Abstract:
This spedification covers six types of plastic media used for removal of organic coatings in an abrasive blast operation.
| Download PDF |
|---|