Peening Media General Requirements AMS 2431 A
Author: SAE
Source: SAE: AMS 2431A, REV 09/01/1996
Doc ID: 1996102
Year of Publication: 1996
Abstract:
This specification and its supplementary detail specifications cover the requirements for media to be used in controlled shop peening of metal parts.
Reference to AMS 2431 with the appropriate slash number on a purchase order constitutes a requirement to conform to the applicable specification in 2.1
|
|---|
| For more information: http://www.sae.org |
|---|