Peening Media Cast Steel Shot, Hard (55 to 62Hrc) AMS 2431 2B
Author: SAE
Source: SAE: AMS 2431/2B Rev. 12/1997
Doc ID: 1997011
Year of Publication: 1997
Abstract:
The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431.
|
|---|