Aluminum Surface Treatment
Author: C. Edward Eckert
Source: US Patent 5,590,703
Doc ID: 1997013
Year of Publication: 1997
Abstract:
A method for removing a surface layer from a solidified body of metal at an elevated temperature to remove surface defects therefrom. The method comprises providing a solidified body having a surface wherein the body can have a temperature greater than 200 degrees F and below the solidus temperature of the metal. The metal surface is contacted with an abrasive material having a particle size in the range of 6 to 300 grit (US Sieve Series). The abrasive material is applied at a flux sufficient to remove a surface layer from the body, the layer having a thickness in the range of 10 to 300 um to provide a surface substantially free of said surface defects.