Sandblast Mask Laminate With Blastable Pressure Sensitive Adhesive
Author: T Komatsu
Source: US Patent 5,989,689
Doc ID: 1999070
Year of Publication: 1999
Abstract:
A sandblast mask laminate useful in sandblasting operations is disclosed. The laminate comprises a photoresist mask layer, a pressure sensitive adhesive composition comprising a non-elastomeric resin and a tackifier in combination to produce a compositionhaving a Tg of less than about -40 degrees C., a carrier film layer and a release liner.