Test Strip Holder, and Gage for Shot Peening
Author: SAE
Source: SAE: J 442 Rev. December 2001
Doc ID: 2001039
Year of Publication: 2001
Abstract:
This SAE Standard defines requirements for equipment/supplies to be used in measuring shot peening intensity. Guidelines for the use of these articles (test strip, holding fixture, and gage) are also included.
|
|---|