Method of Shot Peening Processing and Article Processed Thereby, and Peening Material and Use Thereof
Author: A.Inoue, J.Kurosaki, K.Okumura, K.Kajita
Source: US Patent 6,658,907 B2
Doc ID: 2003008
Year of Publication: 2003
Abstract:
ABSTRACT
A method for shot peening wherein peening shot having a Vickers hardness (Hv) in the range of 900-1100 and a Young's modulus of 200,000 MPa or less, is used, and wherein a treated article is obtained by such a method that has a maximum residual compressive stress of 1600 MPa or more and a surface roughness of 5 microns or less.