High Carbon Cast-Steel Shot
Author: SAE
Source: SAE: J 827 JUL2005
Doc ID: 2005042
Year of Publication: 2005
Abstract:
This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning operations.
|
|---|