Peening Media Glass Shot AMS 2431/6B
Author: SAE
Source: SAE: AMS 2431 6B 02/2005
Doc ID: 2005134
Year of Publication: 2005
Abstract:
This specification, in conjunction with the general requirements covered in AMS 2431 establishes the requirements for glass shot to be used for peening of metal parts.
|
|---|