Peening Media (AWRC) Conditioned Carbon Steel Cut Wire Shot, Hard (45 to 52Hrc) AMS 2431 3C
Author: SAE
Source: SAE: AMS 2431/3C, REV 02/2002
Doc ID: 2006039
Year of Publication: 2006
Abstract:
AMS 2431/3C is a Five Year Review and update for this specification.
|
|---|