Peening Media General Requirements
Author: SAE
Source: SAE: AMS 2431B 05/2006
Doc ID: 2006042
Year of Publication: 2006
Abstract:
The complete requirements for procuring the product shall consist of this document and the latest issue of the basic specification, AMS 2431.
|
|---|