Shot Peening, Automatic
Author: SAE
Source: SAE: AMS 2430 N Rev. 06/2008
Doc ID: 2008028
Year of Publication: 2008
Abstract:
This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
|
|---|