Discussion on Intensity and Coverage
Author: Jack Champaigne
Source: Education Division of Electronics Inc
Doc ID: 2008040
Year of Publication: 2008
Abstract:
Confusion over separation of the concepts "Intensity" and "Coverage" (or "Cycle Time") is often
encountered as a problem in the shot peening industry. Consequently SAE Committee (Fatigue
Design and Evaluation) decided to remove references to coverage from SAE J443 Procedures for
Using Standard Shot Peening Test Strip and created a new document SAE J2277, "Shot Peening
Coverage" issued in January of 2003.