Shot Peening, Automatic
Author: SAE
Source: SAE: AMS 2430 P Rev. 03/2009
Doc ID: 2009008
Year of Publication: 2009
Abstract:
This specification covers the engineering requirements for automatic peening of surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
|
|---|