Computer Generated Shot Peening Saturation Curves
Author: SAE
Source: SAE: J2597 Jan 2010
Doc ID: 2010001
Year of Publication: 2010
Abstract:
The purpose of this recommended practice is to provide an objective method of determining the intensity of peening from a saturation curve. SAE J443 provides instructions for use of the test strip and a review of that document illustrates the need for a standardized procedure.
|
|---|